Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3WC4 - PA66-CF20 - BASF

Material Data Center offers the following functions for Ultramid® A3WC4:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
以20 %碳纤维增强的导电性等级。 用于机械元件和具有高刚度、 尺寸稳定性、 低密度与良好摩擦特性的外壳 (例如连杆)。
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 10 / * cm³/10min ISO 1133
温度 275 / * °C -
载荷 5 / * kg -
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 17000 / 12000 MPa ISO 527
断裂应力 230 / 160 MPa ISO 527
断裂伸长率 2.5 / 6 % ISO 527
拉伸蠕变模量, 1h * / 8000 MPa ISO 899-1
拉伸蠕变模量, 1000h * / 6800 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C 60 / 70 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 50 / - kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 11 / 16 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 7.5 / - kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 260 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 245 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 250 / * °C ISO 75-1/-2
线性热膨胀系数, 平行 9 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 86 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.6 / * mm -
Yellow Card 现存 是的 / * - -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
Yellow Card 现存 是的 / * - -
电性能干 / 已调节单位Test Standard
ISO数据
体积电阻率 86000 / - Ohm*m IEC 62631-3-1
介电强度 5 / 5 kV/mm IEC 60243-1
相对漏电起痕指数 - / 100 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 6.5 / * % 类似ISO 62
吸湿性 2 / * % 类似ISO 62
密度 1220 / - kg/m³ ISO 1183
模塑测量的特殊性能干 / 已调节单位Test Standard
ISO数据
粘数 150 / * cm³/g ISO 307, 1157, 1628
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 4 h -
加工湿度 ≤0.15 % -
注塑熔体温度 280 - 300 °C -
模具温度 80 - 90 °C -
函数
动态剪切模量-温度 , Ultramid® A3WC4 (烘干), PA66-CF20, BASF
应力-应变.  , Ultramid® A3WC4 (烘干), PA66-CF20, BASF
正割模量-应变.  , Ultramid® A3WC4 (烘干), PA66-CF20, BASF
应力-应变(等时的) 23°C, Ultramid® A3WC4 (状况), PA66-CF20, BASF
蠕变模量-时间. 23°C, Ultramid® A3WC4 (状况), PA66-CF20, BASF
蠕变曲线 23°C, Ultramid® A3WC4 (状况), PA66-CF20, BASF
应力-应变(等时的) 90°C, Ultramid® A3WC4 (烘干), PA66-CF20, BASF
蠕变模量-时间. 90°C, Ultramid® A3WC4 (烘干), PA66-CF20, BASF
蠕变曲线 90°C, Ultramid® A3WC4 (烘干), PA66-CF20, BASF
应力-应变(等时的) 120°C, Ultramid® A3WC4 (烘干), PA66-CF20, BASF
蠕变模量-时间. 120°C, Ultramid® A3WC4 (烘干), PA66-CF20, BASF
蠕变曲线 120°C, Ultramid® A3WC4 (烘干), PA66-CF20, BASF
拉伸模量-温度 , Ultramid® A3WC4 (烘干), PA66-CF20, BASF
典型数据
加工方法
注塑
供货形式
粒料
添加剂
润滑剂, 脱模助剂
特殊性能
提高导电性, 经热稳处理的/耐热的
地区供应
欧洲
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.